Why Does Liquid Epoxy Solidify in Winter? โ€” Resin Crystallization

๐Ÿ’ก In This Article

  • What is going on when a liquid epoxy hardens without curing
  • What happens when a high-purity resin meets a cold season
  • How to tell crystallization, cure, and whitening apart in the field
  • What traces remain if a crystallized resin is used as it is

In the previous article, Why Do Different Epoxy Resins Behave So Differently? โ€” Reading Epoxy Resins by Their Molecular Structure, I briefly mentioned that a symmetric, high-purity liquid resin turns cloudy and solid in the cold. This article is about exactly that: crystallization.

In winter, you open a pail of resin and the contents have turned cloudy, or white granules have settled at the bottom, or in the worst case the whole pail has set like wax. No hardener was added, yet it is solid, and the first time you see it, it is easy to be alarmed. Has the resin gone bad? Has it started to cure? Should it be thrown out, or can it be used as it is? The short answer is that in most cases it has neither gone bad nor cured. That does not mean it can be used as it is, though. In this article, we look at why crystallization happens, how to tell it apart from cure and other phenomena, and how to handle a crystallized resin.

It Solidified, but It Isn’t Cure

A crystallized liquid epoxy typically looks like one or more of the following:

  • Resin that was transparent turns cloudy (fine crystals suspended in it)
  • White granules or lumps of crystal form on the bottom or walls of the pail
  • Viscosity becomes abnormally high, and in severe cases the whole pail turns white and solid
  • In a two-component adhesive, only the resin (Part A) has solidified, while the hardener (Part B) is fine

The biggest difference from cure is that it is reversible. Cure is an irreversible reaction in which the epoxy groups react with the curing agent and the molecules link chemically. Once it hardens, it never melts again. Crystallization is a physical change of state in which molecules line up in an orderly way without any chemical bonding. Just as ice becomes water again when it melts, a crystallized resin returns to its original transparent liquid when it is warmed appropriately.

Crystallization versus cure (schematic). Crystallization: molecules line up regularly without chemical bonds โ†’ returns to a liquid when heated (reversible). Cure: molecules bond chemically with the curing agent to form a network โ†’ does not melt when heated (irreversible).

Liquid Epoxy Is Actually a “Supercooled Liquid”

To understand crystallization, you first need to know one surprising fact. The liquid bisphenol A epoxy resin we use every day at room temperature is, strictly speaking, a substance that should be a solid but is staying in the liquid state. In the previous article, I said that the properties of a bisphenol A resin depend on the repeat unit (n). If you collect only the shortest molecule, with no repeat unit (n = 0), in pure form, it is a crystalline solid with a melting point of about 40 ยฐC. In other words, room temperature is below this substance’s melting point. A liquid resin can exist as a liquid at room temperature only because the process by which molecules line up and form crystals is very slow. This state, in which a material remains a liquid below its melting point without forming crystals, is called supercooling.

A supercooled liquid looks stable on the surface but is always ready to become a crystal. Becoming a crystal takes two steps:

  • Nucleation: a few molecules line up for the first time and form the “seed” of a crystal
  • Growth: molecules attach one after another around the seed, and the crystal gets bigger

The hard part is the first step. Once a seed exists, it grows relatively easily from then on. That is why crystallization appears as something that “you can’t predict when it will happen, but once it starts, it spreads quickly.” It is also why a resin that was perfectly fine yesterday can set solid through the whole pail within a few days.

How crystals form in a supercooled liquid (schematic). Supercooled liquid โ†’ seed (nucleus) forms โ†’ crystal grows around the seed โ†’ spreads through the whole container.

Why High Purity, and Why Winter

The conditions under which crystallization occurs readily can be sorted into three groups.

โ‘  The higher the purity. I said in the previous article that molecules of the same shape line up easily. The higher the proportion of n = 0 molecules in a liquid resin, that is, the more uniform the molecular size, the easier the lining up. This is why high-purity grades with low epoxy equivalent weight and low viscosity, and grades that have been purified by distillation, are especially prone to crystallization. Conversely, if molecules with different repeat units are mixed in, or a resin of a different shape such as bisphenol F is blended in, the lining up is disturbed and crystallization is delayed. High purity is an advantage in terms of quality but a weakness in terms of crystallization.

โ‘ก When it is moderately cold, and when the temperature swings. The lower the temperature is below the melting point, the stronger the drive to crystallize. But if it is too cold, viscosity rises sharply and the molecules cannot move, so crystals actually do not grow well. Crystallization therefore tends to be most active at a moderately cool temperature, not in extreme cold. An unheated warehouse or a logistics chain in winter is just such an environment. Temperature swings add to the risk. In an environment that is warm by day and cold at night, small seeds formed in the cold may not melt completely when it is warm, and remain to grow larger in the next cold spell. That is why a place with a large day-night temperature difference is more dangerous than a place that is consistently cool.

โ‘ข When there is something to serve as a seed. Nucleation happens much more readily where there is something to hold on to than where there is nothing. Dust, scratches on the container wall, foreign matter that got in, and filler particles can all act as seeds. A developer should remember that a filled formulation can be more prone to crystallization than the neat resin. Also, if a resin that crystallized earlier is used without melting it completely, invisible fine crystals remain and crystallization starts again quickly.

Cure, Crystallization, or Whitening?

When a resin or adhesive turns white or hard in the field, the first thing to do is to work out what it is. The appearance may be similar, but the cause and the response are completely different.

CrystallizationCure (Gelation / Premature Cure)Amine Blush (Whitening)Filler Settling
Where it occursMostly in the resin (Part A) aloneThe mixture, or a one-component adhesiveThe cured surfaceThe bottom of a filled formulation
When heatedMelts and becomes clearDoes not meltNo changeNo change
In solvent (acetone, etc.)DissolvesDoes not dissolve (swells)Only the surface layer is washed offRedisperses when mixed
By DSCEndothermic peak near the melting pointNo melting peak; residual exotherm decreasesโ€”โ€”
Main causeCold storage, high purity, temperature swingsReaction proceedingReaction of amine with moisture and COโ‚‚Density difference, low viscosity

The simplest way to tell is to take a small amount and warm it. If it is crystallization, warming above the melting point returns it to a clear liquid. If it does not melt when warmed and even gets harder, the reaction has proceeded, and it is not crystallization. If you have analytical equipment, DSC gives a definitive answer. Crystals absorb heat when they melt, so an endothermic peak appears near the melting point, while the cure reaction shows up as an exothermic peak. (See: Why Does Epoxy Turn White? โ‘  โ€“ Whitening Caused by Processing and Material Factors)

Can a Crystallized Resin Be Used as It Is?

Crystallization is reversible, so the resin itself has not gone bad. But using it while crystals remain is risky, for two reasons.

โ‘  The mix ratio goes off. Crystals form mostly from n = 0 molecules. As crystals form, the remaining liquid has fewer n = 0 molecules and a higher proportion of longer molecules. In other words, the epoxy equivalent weight of the crystal portion and that of the liquid portion differ. If you scoop out only the liquid portion, or weigh out resin with crystals mixed in, the actual epoxy equivalent weight differs from the design value, and the ratio to the hardener goes off. As I have said repeatedly in earlier articles, a mix ratio that is off leads to incomplete cure or degraded properties.

โ‘ก Traces remain in the cured material. If the resin is cured with undissolved crystals in it, the crystal portion hardens without mixing properly with the hardener. As a result, white spots or localized undercure can remain in the cured material. These spots can look like foreign matter or whitening and lead you to look for the cause in the wrong place. In a dispensing process, crystal granules can also clog the nozzle.

So a crystallized resin should be used only after it has been completely melted. The usual method is as follows:

  1. Warm the container to a temperature well above the melting point (usually around 50โ€“60 ยฐC, but the manufacturer’s recommended conditions take priority).
  2. Melt it completely until no crystals are visible, then stir well until uniform.
  3. Cool it to room temperature before mixing with the hardener. (Mixing while hot greatly shortens the pot life.)

“Completely” is important here. If you stop warming because most of it looks melted, the fine crystals left over become seeds and the resin crystallizes again quickly. There is one more caution: this method applies only to resin with no hardener mixed in. If you warm a one-component adhesive that already contains a latent hardener, the cure reaction may start instead of the crystals melting. For one-component adhesives, always follow the manufacturer’s instructions. (See: Why Are One-Component Epoxy Adhesives Stored in a Refrigerator (or Freezer)?)

Preventing Crystallization

Once crystallization occurs, melting the resin takes effort, and using it unknowingly leads to defects. Preventing it beforehand is best.

Storage

  • In winter, store the resin in a heated place at a steady temperature.
  • Avoid places with a large day-night temperature difference, such as near doors or against exterior walls.
  • Check for crystals at receiving, and do not leave stock piled up for a long time; use first in, first out.
  • Close the container well after use so that dust and foreign matter do not get in.

Formulation

  • If crystallization is frequent, consider a crystallization-resistant grade, or a grade that blends bisphenol A and F types.
  • As we saw in the previous article, mixing molecules of different shapes disturbs their lining up.
  • A filled formulation can behave differently in terms of crystallization, so check beforehand with a low-temperature storage test.

Conditions that invite crystallization and ways to prevent it (schematic). Conditions that invite it: high purity, cool temperature, temperature swings, seeds (dust, filler, residual crystals). Ways to prevent it: storage at a steady temperature, blended grades, complete melting before use, keeping out foreign matter.

Summary

ItemKey Point
What it isA physical change of state, not cure. Returns to a liquid when heated
PrincipleLiquid epoxy is a supercooled liquid that stays liquid below its melting point
Conditions that favor itHigh purity, moderately cool temperature, temperature swings, seeds (dust, filler, residual crystals)
How to tellIt melts when warmed, it dissolves in solvent, and DSC shows an endothermic peak
If used as it isEpoxy equivalent weight goes off and the mix ratio is wrong; spots and localized undercure in the cured material
What to doMelt completely, stir, cool, then use. For one-component adhesives, do not warm; check the manufacturer’s instructions

A Development Note: If It’s Already Dissolved, It Can’t Solidify

For preventing crystallization, I described storage temperature and formulation above, but the method I actually used in the field was a little different. For a resin that crystallizes easily, I kept it from the start as a solution dissolved in solvent, and when formulating, I weighed it out allowing for the proportion of that solution.

The principle is similar to sugar water. Sugar can be dissolved in water only up to a limit, and crystals reappear only when that limit is exceeded. The same is true of resin. When it is dissolved in a solvent, the resin concentration is lower, and it becomes hard to exceed the limit (the solubility) at the storage temperature. If you do not exceed the limit, there is no reason to crystallize in the first place. Solvent molecules also get in between the resin molecules and disturb their lining up. And the trouble of warming the pail every winter and checking that all the crystals have melted disappears.

Of course, this method does not work in every case. It is possible only when the final product is a solvent-based formulation, and it cannot be used for a solvent-free one. Keeping the resin as a solution also adds one more thing to watch: the solids content. You need to know exactly how much resin is in the solution so that you can convert the epoxy equivalent weight to a solids basis and set the hardener ratio. If solvent evaporates little by little as the container is opened and closed, the solids content changes, and at the mouth or walls of the container, where concentration rises, crystals can actually form instead. Container management and checking the solids content therefore have to go with it. It turned the problem of crystallization into a different management item, solids control, but that was a much easier thing to manage than warming and melting the pail every time.

Final Thoughts

In this article, we saw that crystallization is a physical change of state and not cure, and that using it without knowing can lead to mix ratio errors or spots in the cured material. Looking back, crystallization was less a problem of the resin itself than one met at the production site that receives the resin and turns it into adhesive.

Most of the articles on this blog so far have been written from the viewpoint of a developer who designs and evaluates adhesives. But a formulation completed in the lab does not become a product right away. The moment comes when a formulation that was mixed in a few hundred grams has to be made in tens or hundreds of kilograms. And many developers are thrown for the first time then. The same raw materials were mixed in the same ratio, so why does what was made in the lab differ from what was made in mass production?

In the next article, Why Doesn’t a Lab Formulation Work as It Is in Mass Production?, we will shift to the viewpoint of production, which actually makes the adhesive, and look at what changes in the scale-up process.

Leave a Reply